EN AW 7049A Alloy

Alloy name: EN AW 7049A
Diagram No.: 782
Type of diagram: CCP
Chemical composition in weight %: 0.25% Si, 0.35% Fe, 1.90% Cu, 0.20% Mn, 2.90% Mg, 0.22% Cr, 8.2% Zn, 0.10% Ti, balance is Al
Alloy group: Aluminium-based alloys
Note: CCP diagram of the EN AW 7049A alloy calculated from the excess cp curves, the marked sighs indicate the start and end temperature of the main exothermic reactions.
In Fig. the CCP diagram represents the main exothermic reactions starting and ending depending on temperature. The violet circles represent the starting of the high temperature reaction, and the pink triangles are the ending of the low temperature exothermic reaction. The limits are close to 4 K/s, which is due to DSC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.