Inconel 718 Alloy

Alloy name: Inconel 718
Diagram No.: 786
Type of diagram: TTT
Chemical composition in weight %: 17.8-19.1% Fe, 0.03-0.06% C, 0.21- 1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-6.17% Nb+Ta, 0.96-1.0% Ti, 0.42-0.47% Al, balance is Ni
Alloy group: Nickel-based alloys
Note: Heat treatment schedule is critical to desired mechanical properties. Oradei-Basile et al.
Reference: Not shown in this demo version. Tom Gallmeyer, Effects of heat treatment on L-PBF Inconel 718, ADAPT Monthly Meeting March 14, 2018, PowerPoint Presentation, pp. 1-26.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.