Ti–43.67Al–4.08Nb–1.02Mo–0.1B Alloy

Alloy name: Ti–43.67Al–4.08Nb–1.02Mo–0.1B
Diagram No.: 790
Type of diagram: CCT
Chemical composition in atomic %: 43.67% Al, 4.08% Nb, 1.02% Mo, 0.1% B, balance is Ti
Alloy group: Titanium-based alloys
Note: Continuous-cooling-transformation (CCT) diagram for the phase precipitation during the heat treatment of a TNM alloy. Broad black lines confine regions in which the given Gamma phase fraction (in m %) is certainly exceeded. The cooling paths plotted as narrow black lines result from the linear cooling rates of 35, 300, 500, 900 and 1200 K/min, respectively. Thus, the influence of technologically relevant cooling rates on the quantitative gain in the Gamma phase can be derived [87]. Actual Gamma phase fractions (in m %) before and after cooling are indicated in the boxes at the bottom. (Reprinted from Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.