6063 Alloy

Alloy name: 6063
Diagram No.: 794
Type of diagram: CCT
Chemical composition in weight %: 0.59% Si, 0.19% Fe, 0.02% Cu, 0.03% Mn, 0.47% Mg, 0.005% Cr, 0.03% Zn, 0.013% Ti, balance is Al
Alloy group: Aluminium-based alloys
Note: Continuous cooling precipitation diagram of the investigated composition of 6063 after solution annealing at 540 C 20 min.
Reference: Benjamin Milkereita, Nelia Wanderka, Christoph Schick, Olaf Kessler, Continuous cooling precipitation diagrams of Al–Mg–Si alloys, Materials Science and Engineering A 550 (2012), pp. 87–96.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.