Al - 0.9% Mn - 0.35% Fe - 0.04% Si Alloy

Alloy name: Al - 0.9% Mn - 0.35% Fe - 0.04% Si
Diagram No.: 8
Type of diagram: TTP
Chemical composition in weight %: 0.9% Mn, 0.35% Fe, 0.04% Si, balance is Al
Alloy group: Aluminum-based alloys
Note: A commercially srip-cast AlMn alloy exhibiting a uniform primary particle structure with a secondary dendrite spacing similar to that reported by Moritn and Ostermann. Heat treatment: Material annealed at 670 (1058 F) for 6 h, then cooled at a rate of about 100C (212 F)/h to 450C (842 F) and kept at thin temperature for an additional period of 41 h. The resulting decrease in reairtivity wan 36%, or about 0.3% Mn in solid rolution. The material wan then reduced 85% at room temperature, and recrystallized at different temperaturea and times.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.