IN-945X Alloy

Alloy name: IN-945X
Diagram No.: 802
Type of diagram: TTT
Chemical composition in weight %: 54.02% Ni, 20.64% Cr, 14.41% Fe, 3.19% Mo, 3.91% Nb, 1.93% Cu, 1.44% Ti, 0.18% Al, 0.06% Mn, 0.05% Si, 0.0008% S, 0.007% P, 0.007% C, 0.002% B, 0.02% W, 0.12% Co
Alloy group: Nickel-based alloys
Note: Time-Temperature-Transformation diagram of alloy 945X. To generate the time-temperature-transformation diagram of Incoloy alloy 945X, alloy specimens were solution heat treated for 1 hour at 1040 C (above solvus temperature) and water quenched for full dissolution of precipitate phases. After solution heat-treating the alloy samples, the test specimens were subjected to isothermal treatment in the temperature range of 650 C to 900 C at 50oC intervals, for 10 minutes to 120 hours and water quenched to hold the constituents and precipitation phases in solution.
Additional links: No. 802, No. 803, No. 804, No. 805
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.