Ni52Ti48 Alloy

Alloy name: Ni52Ti48
Diagram No.: 814
Type of diagram: TTT
Chemical composition in weight %: Ni52Ti48
Alloy group: Nickel-based alloy
Note: TTT diagram describing aging behavior for Ni52Ti48 alloy. Rapid cooling of NiTi with addi>onal low-temp aging will exclusively nucleate Ni4Ti3. (Metastable) Ni4Ti3 -> Ni3Ti2 -> Ni3Ti (Equilibrium). How will hafnium addi>on change the TTT curve?
Reference: Not shown in this demo version. Sean Mills, Aaron Stebner, Christopher Dellacorte, Ronald D. Noebe, Jonathan Almer, Jun-Sang Park, Development of Advanced Nickel-Titanium-Hafnium Alloys for Tribology Applications, Poster, 2017, http://hdl.handle.net/11124/170886 http://dx.doi.org/10.25676/11124/170886.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.