RR2071 Alloy

Alloy name: RR2071
Diagram No.: 840
Type of diagram: TTP
Chemical composition in weight %: 62.0% Ni, 9.50% Co, 6.60% Cr, 4.50% Mo, 0.00% W, 2.80% Re, 5.60% Al, 1.30% Ti, 7.30% Ta, 0.30% Nb, 0.10% Hf
Alloy group: Nickel-based alloys
Note: TTT curve for the formation of TCPs including backscattered electron SEM micrographs showing the morphology of the phases. Figure shows the experimentally determined TTT curve for the onset of the formation of TCPs in RR2071. TCPs are apparent after 20 hours annealing times at temperatures of 1000C -1050C. but are not observed after prolonged annealing at 1150C.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.