AA6063 Alloy

Alloy name: AA6063
Diagram No.: 854
Type of diagram: TTT
Chemical composition in weight %: max. 0.1% Cr, max. 0.1% Cu, max. 0.35% Fe, 0.45-0.9% Mg, max. 0.1% Mn, max. 0.15% Others, 0.2-0.6% Si, max. 0.1% Ti, max. 0.1% Zn, balance is Al
Alloy group: Aluminium-based alloys
Note: Schematic TTT curves for Mg2Si precipitation in AA6063 [redrawn from Sheppard’s diagram [5]. Figure shows a schematic TTT (time-temperature-transformation) diagram indicating the precipitation sequence during cooling of dilute Al-Mg-Si alloys of the AA6063 type, and shows that the Mg2Si precipitate can take two forms, one occurring in an upper temperature range (Beta) and the other in a lower range (Beta’). In contrast, the Beta’ metastable phase, which forms at lower temperature, tends to be bounded by partially coherent interfaces and due to nature of their low mobility, limit the rate of precipitate dissolution.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.