Al - 2.7% Cu - 1.6% Li - 0.09% Zr - 0.05% Fe - 0.05% Si - 0.10% Ti Alloy

Alloy name: Al - 2.7% Cu - 1.6% Li - 0.09% Zr - 0.05% Fe - 0.05% Si - 0.10% Ti
Diagram No.: 9
Type of diagram: TTP
Chemical composition in weight %: 2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.05% Si, 0.10% Ti, balance is Al
Alloy group: Aluminum-based alloys
Note: Panels of the 3.5 mm thick section were taken from the midthickness of the plate and solution treated at 550C (1022 F) for 3O min in molten metal, then transferred to molten metal baths operating at either 500, 450, 400, 350 or 300C (932, 842, 752, 662, or 572 F) for timer ranging to 10,000 s. They were then quenched in cold water.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.