Pd43Ni10Cu27P20 Alloy

Alloy name: Pd43Ni10Cu27P20
Diagram No.: 901
Type of diagram: CCH
Chemical composition in weight %: Pd43Ni10Cu27P20
Alloy group: Palladium-based glass
Note: Continuous cooling and heating CCH diagram of Pd43Ni10Cu27P20. In this diagram the cumulative time during constant heating and cooling from the glass transition temperature and the equilibrium liquid, respectively, is plotted vs temperature. Open circles denote the onset of crystallization for unfluxed samples cooled from the equilibrium melt and solid circles for the fluxed samples. The onset of crystallization for fluxed samples heated from the amorphous state is shown by solid diamonds (solid romb) and open diamonds (open romb) denote the onset of crystallization measured on unfluxed samples. The critical cooling rate of 0.09 K/s and the critical heating rate of approximately 6 K/s for the fluxed Pd43Ni10Cu27P20 are denoted by the dashed and solid line, respectively.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.