Inconel 625 Alloy

Alloy name: Inconel 625
Diagram No.: 902
Type of diagram: TTT
Chemical composition in weight %: max. 0.10% C, 20.0-23.0% Cr, 8.0-10.0% Mo, max. 5.0% Fe, max. 0.015% P, max. 0.5% Si, max. 0.015% S, max. 0.50% Mn, Cb+Ta: 3.15-4.15%, max. 0.40% Al, max. 0.40% Ti, balance is Ni
Alloy group: Nickel-based alloys
Note: Experimentally determined TTT diagram for L-PBF IN625 [3,5] The curves represent the time-temperature combinations that result in a volume fraction of ~ 1% Delta phase in AM IN625 (red solid line) compared to wrought IN625 (black dashed line), from Ref. [9] (Color figure online). L-PBF - Laser powder-bed fusion.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.