718 Alloy

Alloy name: 718
Diagram No.: 912
Type of diagram: TTT
Chemical composition in weight %: 17.8-19.1% Fe, 0.03-0.06% C, 0.21- 1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-6.17% Nb+Ta, 0.96-1.0% Ti, 0.42-0.47% Al, balance is Ni
Alloy group: Nickel-based alloys
Note: (a) Experimentally observed [30] and calculated [10] TTT diagram for alloy 718.
Figure shows the calculated TTT diagram [10] for a 718 alloy and compares it with experiment [30]. In this case the Gamma', Gamma'' and Delta phases are considered from the solution temperature, while Sigma forms from transformed Gamma at the temperature of calculation. For alloys of this type, the CCT diagram is often of equal importance and it is possible to convert a TTT diagram to a CCT diagram using well-known additivity rules.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.