Zr55Al22.5Co22.5, Zr57Cu15.4Ni12.6Al10Nb5, Zr41.2Ti13.8Cu12.5Ni10Be22.5 Alloys

Alloy name: Zr55Al22.5Co22.5, Zr57Cu15.4Ni12.6Al10Nb5, Zr41.2Ti13.8Cu12.5Ni10Be22.5
Diagram No.: 936
Type of diagram: TTT
Chemical composition in weight %: Zr55Al22.5Co22.5, Zr57Cu15.4Ni12.6Al10Nb5, Zr41.2Ti13.8Cu12.5Ni10Be22.5
Alloy group: Zirconium-based metallic glass
Note: TTT fitting curves for the three alloys with temperature axis normalized by the glass transition temperature (Tg). In order of increasing nose times, the TTT curves correspond to Zr55Al22.5Co22.5 (ZrAlCo), (Vit106), and Zr41.2Ti13.8Cu12.5Ni10Be22.5 (Vit1). The secondary y-axis shows the dynamic viscosities of the three alloys at the nose temperature of the TTT curves. Error bars in viscosity of 20% are shown. The viscosity scales linearly with the crystallization time at the nose temperature.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.