41.5% SiO2 - 33.9% Ca0 - 24.6% Al2O3

Name: 41.5% SiO2 - 33.9% Ca0 - 24.6% Al2O3
Diagram No.: 963
Type of diagram: TTT
Chemical composition in weight %: 41.5% SiO2, 33.9% Ca0, 24.6% Al2O3
Group: Slags
Note: Crystallization behaviour for the composition 41.5% SiO2 - 33.9% Ca0 - 24.6% Al2O3 TTT diagram (a); proportions of anorthite CAS2(b).
Atypical exampleof a diagram showing the transition glassy/crystallized (TTT curves) for a composition of the CaO-Si02-Al203 system located in the primary phase field of anorthite is given in Fig. Only anorthite crystals have appeared, for the holding times considered, in amounts shownon the samefigure, for the temperature of 1154 C. It is interesting to note that the limiting amount of anorthite crystals obtained is very close to the evaluation for the metastable system liquid oxide/anorthite at 1154 C, calculated using the exploitation programs of IRSID slag model, which predicts 46% anorthite.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.