CaO–SiO2–TiO2 Slag

Alloy name: CaO–SiO2–TiO2 Slag
Diagram No.: 969
Type of diagram: TTT
Chemical composition in weight %: See the table
Alloy group: Slags
Note: CCT diagrams of (a) glass CST and (b) glass CS.
Figure (a) illustrates the CCT diagram of glass CST. Closed circles, opened triangles and opened squares represent Peak 1, Peak 2 and Peak 3, respectively. The line connected the closed circles expresses the crystallization of CaOSiO2 and the line connected the opened triangles expresses the crystallization of CaOSiO2TiO2.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

969969 Crystallization temperature and crystallization time of DTA measurement

969-2969-2 Click the table to enlarge the data.

Results of X-ray diffraction studies and microstructure observation by EPMA

969-3969-3 Click the table to enlarge the data.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.