Ti–BF slag

Name: Ti–BF slag
Diagram No.: 981
Type of diagram: TTT
Chemical composition in weight %: See the tables 1 and 2
Group: Slags
Note: Figure displayed the TTT diagrams of the samples. It was found that the incubation time decreased with the addition of TiO2 at the same basicity, and the higher basicity of the samples was, the smaller influence of the TiO2 addition on the crystallization would be, which indicated that the addition of TiO2 was more beneficial to the crystallization of the slags at lower basicity. It was also observed that the incubation time initially increased and then decreased with increasing the basicity at the same TiO2 content, which may suggest that the crystallization was firstly inhibited and then promoted with the basicity increasing at the same TiO2 content.
Moreover, it was seen that the TTT diagram of slag No. 4, No. 6, No. 9 and No. 12 showed double-C shape, which may imply the different crystals formed or the change of the crystallization mechanism at different temperatures in the samples.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.