Allvac 718Plus Alloy

Alloy name: Allvac 718Plus
Diagram No.: 992
Type of diagram: TTT
Chemical composition in weight %: 0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, balance is Ni
Alloy group: Nickel-based alloys
Note: TTT Curves of Gamma' and Gamma" Precipitation in Alloy 718Plus Generated by Modeling (Solid Line) and Experiment (Dash Line).
A TTT curve of Gamma’ and Gamma’’ phases was calculated by JMatPro, as shown in Figure, which also shows the TTT curve of Gamma’/Gamma’’ precipitation determined by hardness measurement on isothermal annealed samples. It can be seen that the precipitation rate of Gamma’ phase is faster than Gamma" phase in this alloy, as it is in alloy 718. Therefore, alloy 718Plus will have faster precipitation kinetics than alloy 718. Gamma prime phase precipitation in this alloy is much slower than Waspaloy however, which has a very high Gamma’ phase precipitation rate.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.


Copyright © 2019 by Steel Data. All Rights Reserved.