Stainless steel-Electrolytic polishing

Material: Stainless steel
Type: Micro
Method: Electrolytic polishing
Etchant (electrolyte): 220 ml water, 200 ml glycerin, 580 ml sulfuric acid.
Procedure: Cell voltage: 1.5-12 V, time: 1-20 min.
Note: Cathode stainless steel.
Source: ASTM E 1559-99: Standard Guide for Electrolytic Polishing of Metallographic specimens, December 1999, p.1-14.