Determining grain structure in A356 aluminum

Material: Determining grain structure in A356 aluminum
Type: Micro
Method: Chemical etching
Etchant (electrolyte): Tuckers reagent: 45ml HCL, 15ml HNO3, 15ml HF, 25ml H2O.
Procedure: No data.
Note: The grain structure will be visible by using a stereo scope (2-4X).
Source: http://www.metallography.com.