Sm-Co alloys-Chemical etching

Material: Sm-Co alloys
Type: Micro
Method: Chemical etching
Etchant (electrolyte): 1-5% nital.
Procedure: No data.
Note: No data.
Source: Fred Hargreaves (Ret.), Personal Etchants Database 1960-1990, Analytical Services Bookham Technology, Caswell, Towcester, Northamptonshire NN8EQ, UK.