Cu-Cr-Zr alloy-Chemical etching

Material: Cu-Cr-Zr alloy
Type: Micro
Method: Chemical etching
Etchant (electrolyte): Ferric chloride.
Procedure: No data.
Note: No data.
Source: V.K.Savin, et al., Met.Trans., Vol.3, No.4, April 1972, p.875.