Al-Cu alloys-Alloys with 10-45% Cu

Material: Al-Cu alloys
Type: Micro
Method: Chemical etching
Etchant (electrolyte): 10% aq. sodium hydroxide.
Procedure: No data.
Note: Alloys with 10-45% Cu.
Source: E.A.Nassef, et al., J.Mat.Sc., Vol.18, No.10, October 1983, p.3031.