Beta alumina-90.4% Al2O3, 8.9% Na2O, 0.7% Li2O

Material: Beta alumina
Type: Micro
Method: Physical etching
Etchant (electrolyte): Thermal etching at 1500 in air.
Procedure: Time: 15 mins.
Note: 90.4% Al2O3, 8.9% Na2O, 0.7% Li2O.
Source: W.I.Archer, et al., J.Mat.Sc., Vol.15, No.8, August 1980, p.2066.