Al-Mg alloy-Alloy with 1-8 at.% Mg

Material: Al-Mg alloy
Type: Micro
Method: Electro polishing
Etchant (electrolyte): 4 parts ethanol, 1 part 60% perchloric acid.
Procedure: Temperature: - 15 C to - 20 C, CD: 0.002 A/mm2, voltage: 3.5 V.
Note: Alloy with 1-8 at.% Mg.
Source: D.Hardie, et al., Phil.Mag. 8th Series, Vol.26, No.4, October 1972, p.897.