Al-Mg-Si alloys-Electro thinning

Material: Al-Mg-Si alloys
Type: Micro
Method: Electro thinning
Etchant (electrolyte): 20% perchloric acid, 80% ethanol.
Procedure: PD: 15-20 V, CD: 0.2 A/cm2, temperature: bellow 30 C.
Note: No data.
Source: R.B.Nicholson, et al., Brit.J.App.Phys., Vol.19, 1958, p.25.