Lenoirs reagent

Material: Lenoirs reagent
Type: Micro
Method: Chemical etching
Etchant (electrolyte): 722 ccs phosphoric acid, 156 gms chromic acid, 136 ccs sulphuric acid, 140 ccs water.
Procedure: No data.
Note: No data.
Source: C.R.Shrasty, et al., Met.Trans., Vol.2, No.12, December 1971, p.3283.