Ni-Cr-Al-Ti-C alloys-10-12% Cr, 5-6% Al, 1% Ti, 0.1% C

Material: Ni-Cr-Al-Ti-C alloys
Type: Micro
Method: Electrolytic etching
Etchant (electrolyte): 5 mls hydrofluoric acid, 10 mls glycerine, 85 mls water.
Procedure: Time: approx. 2 secs, PD: 3 V.
Note: 10-12% Cr, 5-6% Al, 1% Ti, 0.1% C.
Source: E.R.Buchanan, et al., Met.Trans., Vol.4, No.8, August 1973, p.1195.