Udimet 700-Stain etch for inclusions

Material: Udimet 700
Type: Micro
Method: Chemical etching
Etchant (electrolyte): 1 part 4% sodium hydroxide aq. solution, 1 part saturated potassium permanganate solution.
Procedure: No data.
Note: Stain etch for inclusions.
Source: C.P.Sillivan, Trans.ASM, Vol.58, No.4, December 1965, p.702.