Pu-Fe-C alloys-Final electrolytic polishing

Material: Pu-Fe-C alloys
Type: Micro
Method: Electrolytic polishing
Etchant (electrolyte): 1.) 2% solution of sulphuric acid in lactic acid. 2.) 1 part lactic acid, 1 part sulphuric acid, 1 part acetic acid.
Procedure: No data.
Note: Final electrolytic polishing.
Source: J.L.Nichols, et al., Symposium on carbides in Nuclear Energy, Narwell, November 1963, Paper A17.