Mg-Li alloy-Alloy with 10.5 at.% Li

Material: Mg-Li alloy
Type: Micro
Method: Chemical polishing
Etchant (electrolyte): 1 part nitric acid, 3 parts ethyl alcohol.
Procedure: Temperature: 0 C.
Note: Alloy with 10.5 at.% Li.
Source: A.Urukami, et al., Acta Met., Vol.18, No.1, January 1970, p.87.
















Copyright © 2014 by Steel Data. All Rights Reserved.