Mn-Se-S system-MnSe-MnS solid solution. To remove disurbed layers

Material: Mn-Se-S system
Type: Micro
Method: Chemical etching
Etchant (electrolyte): 1% sulphuric acid, 1% phosphoric acid, 1% saturated oxalic acid solution.
Procedure: Mount in bakelite or solder. Polish mecahnically by standard means.
Note: MnSe-MnS solid solution. To remove disurbed layers.
Source: P.E.Riewald, et al., J.Am.Cer.Soc., Vol.52, No.7, July 1969, p.370.
















Copyright © 2014 by Steel Data. All Rights Reserved.