Gadolinium molybdate (Beta-Gd2(MoO4)3)-Chemical etching

Material: Gadolinium molybdate (Beta-Gd2(MoO4)3)
Type: Micro
Method: Chemical etching
Etchant (electrolyte): Etch on C.face with hydrochloric acid for 10 secs or nitric acid for 45 secs (footnotes quote 40% HNO3 and 1 HNO3: 3 H2O).
Procedure: No data.
Note: Polish to 0.3 µm, 0.1 µm alumina.
Source: A.S.Bhalla, J.Electrochem.Soc., Vol.119, No.11, November 1972, p.1602.