C as single crystal graphite specimens-Gas oxidation

Material: C as single crystal graphite specimens
Type: Micro
Method: Gas oxidation
Etchant (electrolyte): x...O2. Note: The volume/quantity was not shown in the referenced article and is therefore designated as an "x".
Procedure: Time: 2 h, temperature: 825 C.
Note: C as single crystal graphite specimens. Oxidation of graphite under the conditions shown produce some evidence of nonbasal dislocations.
Source: Thomas, J M et al. - Phil Mag, 10,325(1964).