In2Te3 specimens-Chemical polishing

Material: In2Te3 specimens
Type: Micro
Method: Chemical polishing
Etchant (electrolyte): 1 part Br2, 19 parts HAc, x...citric acid (Saturate the solution). Note: The volume/quantity was not shown in the referenced article and is therefore designated as an "x".
Procedure: No data.
Note: In2Te3 specimens. Solution used as a polishing etch. After etching, use solution - without bromine to quench reaction and remove residual bromine. Irving, B A, The Electrochemistry of Semiconductors, Holmes, P J, Ed, Academic Press, New York, 1962.
In2Te3 single crystal ingot grown in a study of new semiconducting compounds.
Source: See the above text.