Germanium-Electrolytic polishing

Material: Germanium
Type: Micro
Method: Electrolytic polishing
Etchant (electrolyte): 590 ml methanol 99.8%, 350 ml 2-butoxy ethanol 99%, 60 ml perchloric acid 60%.
Procedure: 30-60 s, 25-35 V DC, stainless steel cathode.
Note:  No data
Source: G. Petzow, Metallographic Etching, 2nd Edition, ASM International, USA, 1999.