Rubidium Sulfide - RbS2

Classification: Sulfide
Atomic numbers: 44 & 16
Atomic weight: 165.82
Melting point (C): >500
Boiling point (C):
Density (g/cm3): 6.99
Refractive index (n=):
Hardness (Mosh-scratch): 7.5
Crystal structure: Isometric-normal: (111) octahedron
Color (solid): Iron-black
Cleavage: Octahedral: (111)