Strontium Fluoride - SrF2

Classification: Fluoride
Atomic numbers: 38 & 9
Atomic weight: 123.67
Melting point (C): 1190
Boiling point (C):
Density (g/cm3):
Refractive index (n=):
Hardness (Mosh-scratch): 1-3
Crystal structure: Isometric-normal: (100) cube
Color (solid): Colorless
Cleavage: Cubic: (001)