Strontium Tungstate - SrWO4

Classification: Tungstate
Atomic numbers: 38, 74 & 8
Atomic weight: 335.55
Melting point (C): 200 del.
Boiling point (C):
Density (g/cm3): 6.187
Refractive index (n=):
Hardness (Mosh-scratch): 3-4
Crystal structure: Tetragonal-pyrimidal: (210) prism
Color (solid): Colorless
Cleavage: Prismatic: (210)