Zinc Selenide - ZnSe

Classification: Selenide
Atomic numbers: 30 & 34
Atomic weight: 144.34
Melting point (C): >1000
Boiling point (C):
Density (g/cm3): 5.42
Refractive index (n=): 2.89
Hardness (Mosh-scratch): 5-6
Crystal structure: Isometric-normal: (100) cube
Color (solid): Grey/yellow
Cleavage: Cubic-perfect: (001)