Cadmium Antimonide - CdSb

Classification: Antimonide
Atomic numbers: 48 & 51
Atomic weight: 234.17
Melting point (C): 1000
Boiling point (C):
Hardness (Mosh-scratch): 6-7
Crystal structure: Isometric-normal: (100) cube
Color (solid): Metallic grey
Cleavage: Cubic: (001)