Zirconium Sulfide - ZrS2

Classification: Sulfide
Atomic numbers: 40 & 16
Atomic weight: 155.34
Melting point (C): >800
Boiling point (C):
Density (g/cm3): 3.87
Refractive index (n=):
Hardness (Mosh-scratch): 4-5
Crystal structure: Hexagonal-normal: (10T0) prism
Color (solid): Steel-grey
Cleavage: Basal-distinct: (0001)