Cadmium Phosphide - CdP2

Classification: Phosphide
Atomic numbers: 48 & 15
Atomic weight: 192.37
Melting point (C): >1000
Boiling point (C):
Density (g/cm3): 4.7
Hardness (Mosh-scratch): 6-7
Crystal structure: Isometric-tetrahedral: (111) tetrahedron
Color (solid): Grey-black
Cleavage: Octahedral: (111)