Cadmium Tellerude - CdTe

Classification: Tellerude
Atomic numbers: 48 & 52
Atomic weight: 240
Melting point (C): 1041
Boiling point (C):
Density (g/cm3): 6.20
Band gap (eV): 1.45
Coefficient of linear thermal expansion (x exp10(-6) cm/cm/C):
Hardness (Mosh-scratch): 5-6
Crystal structure: Isometric-tetrahedral: (111) tetrahedron
Color (solid): Black
Cleavage: Cubic-distinct: (001)