Calcium Molybdate - CaMoO4

Classification: Oxide
Atomic numbers: 20, 42 & 8
Atomic weight: 200
Melting point (C): 1200
Boiling point (C):
Density (g/cm3): 4.35
Refractive index (n=): 1.974-1.984
Coefficient of linear thermal expansion (x exp10(-6) cm/cm/C):
Hardness (Mosh-scratch): 3-3.5
Crystal structure: Tetragonal-normal: (111) pyramid
Color (solid): Yellowish
Cleavage: Basal: (001)