Copper Phosphide - Cu3P

Classification: Phosphide
Atomic numbers: 29 & 15
Atomic weight: 221.73
Melting point (C): cca. 1200
Boiling point (C):
Density (g/cm3): 6.4-6.8
Refractive index (n=):
Hardness (Mosh-scratch): 6-7
Crystal structure: Isometric-normal: (100) cube
Color (solid): Grey/black
Cleavage: Cubic: (001)