Gallium Oxide - Ga2O3

Classification: Oxide
Atomic numbers: 31 & 8
Atomic weight: 187.44
Melting point (C): 1900
Boiling point (C):
Density (g/cm3): 6.44
Refractive index (n=):
Hardness (Mosh-scratch): 5-6
Crystal structure: Hexagonal-trigonal pyramid: (10T1) rhomb, monoclinic: (hkO) prism
Color (solid): White
Cleavage: Basal-poor: (0001)/(001)