Gallium Selenide - GaSe

Classification: Selenide
Atomic numbers: 31 & 34
Atomic weight: 148.68
Melting point (C): 960
Boiling point (C):
Density (g/cm3): 5.03
Refractive index (n=):
Hardness (Mosh-scratch): 6-7
Crystal structure: Hexagonal-normal: (10T0) prism
Color (solid): Steel grey
Cleavage: Basal: (0001)