Germanium Selenide - Ge2Se3

Classification: Selenide
Atomic numbers: 32 & 34
Atomic weight: 181.08
Melting point (C): 900
Boiling point (C):
Density (g/cm3):
Refractive index (n=):
Hardness (Mosh-scratch): 4-5
Crystal structure: Isometric-normal: (100) cube
Color (solid): Clear/grayish
Cleavage: Cubic: (001)