Barium Tungstate - BaWO4

Classification: Oxide
Atomic numbers: 56, 74 & 8
Atomic weight: 385.28
Melting point (C): 1200 approx.
Boiling point (C):
Density (g/cm3): 5.04
Hardness (Mosh-scratch): 4-5
Crystal structure: Tetragonal-pyramidal: (111) pyramid
Color (solid): Clear to whitish
Cleavage: Octahedral: p(111)